mseashell gold fingers/plating on edges... 12-21-2013, 05:05 PM
BRASSCATCHER I would think they would but... 12-21-2013, 05:16 PM
etack The edge plating is thin and... 12-21-2013, 06:18 PM
mseashell Alrighty then. Never knew... 12-21-2013, 06:40 PM
Mechanic688 I believe that jghilino has... 12-21-2013, 06:11 PM
jghilino pm me :D 12-21-2013, 06:16 PM
BRASSCATCHER Etack do those numbers hold... 12-22-2013, 07:21 AM
etack Some boards with full GP... 12-22-2013, 07:10 PM
mseashell Etack what would u say the... 12-22-2013, 03:46 PM
EcoSafe does this mean all fingers... 12-22-2013, 04:26 PM
  1. #10
    EcoSafe's Avatar
    SMF Badges of Honor



    Member since
    May 2011
    Posts
    3,703
    Thanks
    3,699
    Thanked 6,779 Times in 1,949 Posts
    does this mean all fingers and or all plug ins are 30 microns, and 24 kt. I know it is in the Archives but that takes time and effort. Too much like work soooo I'll just ask here.

    Last edited by EcoSafe; 12-22-2013 at 04:31 PM.
    "anyone who thinks scrappin is easy money ain't doin it right!"

  2. The Following User Says Thank You to EcoSafe for This Post:


Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

 
Browse the Most Recent Threads
On SMF In THIS CATEGORY.





OR

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  

The Scrap Metal Forum

    The Scrap Metal Forum is the #1 scrap metal recycling community in the world. Here we talk about the scrap metal business, making money, where we connect with other scrappers, scrap yards and more.

SMF on Facebook and Twitter

Twitter Facebook